MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Materion AuSn Plus Modified Gold-Tin Solder  (discontinued **)
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Solder/Braze Alloy

Material Notes: Developed for RoHS-compliant electronics. The addition of indium to traditional AuSn 80/20 raises its melting point from 278°C to 306°C, providing protection against secondary reflow, loss of hermeticity, or critical component shift during the SMT soldering process. AuSn Plus has comparable physical properties to AuSn and slightly higher processing temperatures near 350°C, similar to those of high-lead solders. The inclusion of indium in the alloy does not affect the AuSn intermetallic formation; the indium substitutes for some of the tin in the Au4Sn intermetallic compound. This ternary alloy is slightly harder and less ductile than traditional AuSn alloy.

Information supplied by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 14.18 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 34.0 ksi
Tensile Strength, Yield 32.5 ksi
Elongation at Break 1.2 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000218 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 55.1 W/m-K
Melting Point 306 °C
Solidus 306 °C
Liquidus 306 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 350 °CPeak

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion Wambraze™ WB280 80Au/20Sn Solder
Indium Corp. Indalloy® 182 Au-Sn Solder Alloy
H.C. Starck WCu 85/15 Tungsten-Copper Composite Material
Gold, Au
Indium Phosphide, InP

NBB9050 / 192313

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.