MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kraiburg TPE THERMOLAST® K TC5FTZ Thermoplastic Elastomer (FR2 Series) Flame Retardant
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The FR2 series is a material solution for applications with high flame retardant requirements. The compounds are halogen-free according to IEC 61249-2-21. The UL94 V-0 (1.5 mm) certificate and the classification according to DIN EN 45545-2 R22/23 HL3 is valid for available hardness range and for natural and colored compounds.

Processing Method: Injection Molding, Extrusion

Color / RAL DESIGN:

  • Natural
  • Black
Typical applications:
  • Gaskets for electric and electronic applications e.g. cable boxes
  • Cable management systems e.g. cable holders, cable glands and grommets
  • Electrical insulation for busbars
  • Applications in railway sector
Material advantages:
  • Halogen-free (according to IEC 61249-2-21)
  • Fulfills railway requirements such as high LOI, low toxicity and smoke density
  • Self-extinguishing, no release of burning droplets
  • Adhesion to PP
  • In-process recycling possible
  • Precoloration in all colors
  • Temperature stability up to 85 °C
  • High glow-wire flammability index (GWFI)
  • No silicones added
  • No interaction with copper
  • Stability in conditions up to 60 °C and 75% humidity

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³DIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050DIN ISO 48-4
Tensile Strength 3.50 MPa508 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 650 %650 %200 mm/min; DIN 53504/ISO 37
Tear Strength 13.5 kN/m77.0 pliISO 34-1 Method B (b)
Compression Set  15 %
@Temperature 23.0 °C,
Time 259000 sec
15 %
@Temperature 73.4 °F,
Time 72.0 hour
DIN ISO 815-1 Method A
 67 %
@Temperature 70.0 °C,
Time 86400 sec
67 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1 Method A
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8260 / 308924

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.