MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Pyro-Bloc® Standard Fibre Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Pyro Bloc modules comprise two sections of Pyrolog slab in edge-grain orientation. These are held in position with two stainless steel tubes mounted transversely through the modules and remote from the hot face. They are anchored to the furnace casing with the patented Pyro Bloc fixing in any one of four standard versions, Y, M, T and Eye-bolt.

Applications: Pyro Blocs have a multitude of uses in heat containment applications in all industry groups, a selection of which are as follows:

  • Petrochemical (process heaters, reformers, pyrolysis heaters and ductwork)
  • Iron and Steel (transfer ladle lids, soaking pit covers, reheating furnace, multi and single stack coil annealing furnaces, continuous annealing and coating furnaces, rotary hearth furnaces, car bottom furnaces, roller furnaces, lift-off furnaces, offtakes and ductwork)
  • Aluminium (soaking pits and covers, bale out furnaces, homogenising furnaces, ductwork)
  • Ceramic (tunnel kilns for whiteware and red brick, intermittent kilns for whiteware and red brick, Hoffman kilns and ductwork)
  • Utilities (thermal oxidisers, waste heat recovery units, combustion chambers and boiler ductwork)

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.160 g/cc0.00578 lb/in³Available Option; Uncompressed
 0.192 g/cc0.00694 lb/in³Available Option; Uncompressed
 0.240 g/cc0.00867 lb/in³Available Option; Uncompressed
Loss On Ignition >= 0.25 %
@Temperature 800 °C,
Time 7200 sec
>= 0.25 %
@Temperature 1470 °F,
Time 2.00 hour
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 2.05 J/g-°C
@Temperature 1000 °C
0.490 BTU/lb-°F
@Temperature 1830 °F
Thermal Conductivity  0.0900 W/m-K
@Temperature 400 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 752 °F
at 240kg/m3; ASTM C-201-68
 0.100 W/m-K
@Temperature 400 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 752 °F
at 192kg/m3; ASTM C-201-68
 0.110 W/m-K
@Temperature 400 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 752 °F
at 160kg/m3; ASTM C-201-68
 0.140 W/m-K
@Temperature 600 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 1110 °F
at 240kg/m3; ASTM C-201-68
 0.160 W/m-K
@Temperature 600 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1110 °F
at 192kg/m3; ASTM C-201-68
 0.180 W/m-K
@Temperature 600 °C
1.25 BTU-in/hr-ft²-°F
@Temperature 1110 °F
at 160kg/m3; ASTM C-201-68
 0.200 W/m-K
@Temperature 800 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 1470 °F
at 240kg/m3; ASTM C-201-68
 0.230 W/m-K
@Temperature 800 °C
1.60 BTU-in/hr-ft²-°F
@Temperature 1470 °F
at 192kg/m3; ASTM C-201-68
 0.250 W/m-K
@Temperature 800 °C
1.74 BTU-in/hr-ft²-°F
@Temperature 1470 °F
at 160kg/m3; ASTM C-201-68
 0.280 W/m-K
@Temperature 1000 °C
1.94 BTU-in/hr-ft²-°F
@Temperature 1830 °F
at 240kg/m3; ASTM C-201-68
 0.310 W/m-K
@Temperature 1000 °C
2.15 BTU-in/hr-ft²-°F
@Temperature 1830 °F
at 192kg/m3; ASTM C-201-68
 0.340 W/m-K
@Temperature 1000 °C
2.36 BTU-in/hr-ft²-°F
@Temperature 1830 °F
at 160kg/m3; ASTM C-201-68
Shrinkage 3.0 %
@Treatment Temp. 1200 °C,
Time 86400 sec
3.0 %
@Treatment Temp. 2190 °F,
Time 24.0 hour
isothermal heating
 
Descriptive Properties
Classification Temperature (°C)1260
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DIAB Klegecell® R 260 Rigid, Closed Cell PVC Foam Core Material
Morgan Advanced Ceramics Pyro-Bloc® Zirconia Fibre Thermal Ceramic
Overview of materials for Acetal Copolymer, PTFE Filled
DuPont Teijin Films Mylar® OL2 Polyester Film, 100 Gauge
DIAB Klegecell® R 130 Rigid, Closed Cell PVC Foam Core Material

CMORF6465 / 203249

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.