MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex APEX® RM 8002 Flexible Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Notes: Apex RM 8002 is a PVC compound generally used in pipe, fitting and appurtenance applications. It is available in green, grey, tan and taupe colors. This compound is NSF/ANSI 61 certified.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Medium Flow, Medium Impact Resistance

Agency Ratings: NSF STD-61

Form: Pellets

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80
@Time 10.0 sec
80
@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 46.4 MPa6730 psiASTM D638
Tensile Modulus 2.81 GPa407 ksiASTM D638
Flexural Modulus 2.76 GPa401 ksiASTM D790
Izod Impact, Notched 1.33 J/cm
@Thickness 3.17 mm
2.50 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C155 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0345 / 236836

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.