Hostacom EYS 2004L W92735 is an unfilled copolymer with high melt flow rate, high gloss, and high scratch resistance. Product is not yet UL certified. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Appliances Market: Electrical / Electronics Attribute: High Gloss Information provided by LyondellBasell. |