MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Palm Labs Adhesives TURBO-LOCK SERIES 16 Anaerobic Thread Locking Compound
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TURBO-LOCK SERIES 16 is a fast curing, GREEN, medium strength, wicking grade, anaerobic thread-locking compound for bonding and sealing threads, and pre-assembled parts. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals. Disassembles with heat and hand tools.

Applications:

  • IPenetrates threads by capillary action. Medium strength thread-locker.
  • Ideal for sealing hairline cracks, small nuts and bolts.
  • Seals and welds porous metal parts. Localize heating and hand tools are needed for disassembly. Prevents corrosion and leakage.
  • Secure setscrews and other assemblies after settings are completed.
  • Fasteners on vibrating machines or moving components.
  • Meets Military specifications:MIL-S-46163 and MIL-S-22473

Part Numbers for this data: 16-001, 16-010, 16-050, 16-250, 16-1000

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 923-26-2, 15625-89-5, 80-15-9 and 114-83-0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/cc
Brookfield Viscosity 12 cP12 cPRVT Spindle 3 @ 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 5.40 MPa>= 783 psiISO 10123; Compressive, Steel pins and collars
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FASTM D696
Specific Heat Capacity 0.300 J/g-°C0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 19.8 min0.330 hourHandling
 60.0 - 180 min1.00 - 3.00 hourFunctional
 1440 min24.0 hourFull
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceGreen
Chemical Resistance50% Initial Strength RetainedMotor Oil at 125°C, at 1000hrs
 85% Initial Strength RetainedBrake Fluid at 22°C, at 1000hrs
 85% Initial Strength RetainedMotor Oil at 125°C, at 500hrs
 90% Initial Strength RetainedGasoline at 22°C, at 500hrs
 90% Initial Strength RetainedBrake Fluid at 22°C, at 500hrs
 90% Initial Strength RetainedWater/Glycol at 87°C, at 500hrs
 90% Initial Strength RetainedWater/Glycol at 87°C, at 1000hrs
 90% Initial Strength RetainedGasoline at 22°C, at 1000hrs
 95% Initial Strength RetainedAcetone at 22°C, at 500hrs
 95% Initial Strength RetainedEthanol at 22°C, at 500hrs
 95% Initial Strength RetainedAcetone at 22°C, at 1000hrs
 95% Initial Strength RetainedEthanol at 22°C, at 1000hrs
CompositionMethacrylate Ester
Torque10 N.mBreakaway, M10 steel nuts and bolts N.m, ISO 10964
 29 N.mPrevail, M10 steel nuts and bolts N.m, ISO 10964
 30 N.mBreakloose, pre-torqued to 5 N.m, M10 steel nuts and bolts, ISO 10964
 40 N.mMax Prevail, pre-torqued to 5 N.m, M10 steel nuts and bolts N.m, ISO 10964

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPALML049 / 135203

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.