Description/Features: - Cadmium-free
- UL 60°C
- Transparent
- Excellent Surface Appearance
- SPT Cord
- Speaker Wire
- Flexible Cords
- Fixture Wire
Applications: - Telecommunication Insulation
- Telecommunication Jacket
Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation. Geon Performance Solutions was created from PolyOne in 2019. |