MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

TPC Group TPC 1105 Enhanced Grade Polyisobutylene
Categories: Polymer

Material Notes: Characteristics: TPC 1105 is colorless (water white), has low moisture transition rates, is non-corrosive, hydrophobic, non-drying and non-staining among other useful properties. TPC 1105 is an Enhanced polyisobutylene (PIB) grade with a viscosity range of 190- 240 cSt and a molecular weight of 1050.

Applications: TPC 1105 can be used for a variety of applications such as: Cosmetics, replacement for bright stocks, mineral oils and process oils, Fuel and Lubricant Oil additive, Emulsifier, 2 stroke engine oil, viscosity modifiers, hot melt adhesives, pour point depressants, tackifiers, PIBSA reactions, emulsions, asphalt/bitumen, elastomer based sealants and caulks, polymer modification, adhesives and cling film.

General: Enhanded PIB grades are used as replacements for conventional grades of PIB. Enhanced PIB grades are ideal for applications where viscosity and tackiness are key qualities of the material. TPC Group offers the broadest portfolio of PIB products to the market and is a major supplier to many different markets, including fuels and lubricants, caulks, sealants, adhesives, packaging, greases and emulifiers.

Packaging: TPC 1105 is typically sold in railcar quantities, but trucks and isocontainers are also available.

Information provided by TPC Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 - 0.910 g/cc
@Temperature 15.6 °C
0.880 - 0.910 g/cc
@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 144144Index; ASTM D2270
Kinematic Viscosity 190 - 240 cSt190 - 240 cStASTM D445
 840 cSt
@Temperature 70.0 °C
840 cSt
@Temperature 158 °F
ASTM D445
 2200 cSt
@Temperature 100 °C
2200 cSt
@Temperature 212 °F
ASTM D445
 5600 cSt
@Temperature 40.0 °C
5600 cSt
@Temperature 104 °F
ASTM D445
 21200 cSt
@Temperature 20.0 °C
21200 cSt
@Temperature 68.0 °F
ASTM D445
Molecular Weight 1050 g/mol1050 g/mol
Evaporation Loss 0.53 %
@Temperature 99.0 °C,
Time 36000 sec
0.53 %
@Temperature 210 °F,
Time 10.0 hour
ASTM D972
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.10<= 0.10[mg KOH/g]; ASTM D974
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown 50000 V50000 VASTM D877
Dissipation Factor 0.000080
@Temperature 100 °C
0.000080
@Temperature 212 °F
ASTM BS5737
 
Thermal PropertiesMetricEnglishComments
Pour Point -6.00 °C21.2 °FASTM D97
Flash Point >= 185 °C>= 365 °FCOC; ASTM D92
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49711.4971ASTM D1218
Haze <= 4.0 %<= 4.0 %Photometric; ASTM D6181
 
Descriptive Properties
AppearanceClear and Bright
Bromine Number15.7 g Br2/100gASTM 1159
Color<50APHA, ASTM D1209
Content<1 ppmChlorine, ASTM D4327
 <1 ppmSulfur, ASTM D2622
 <1 ppmAromatics
 25 ppmWater, ASTM D1533
Power Factor8E-05100°C, ASTM D924
Saponification Number<1 mg KOH/gASTM D94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTPCG007 / 320509

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.