MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polyplastics TOPAS® 6013M-07 Cyclic Olefin Copolymer (COC)
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: TOPAS® 6013M-07 is an injection molding grade with a wide processing window, especially suited for blow molding processes including IBM and ISBM. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface making it an excellent choice for healthcare and other high-tech products. Lower leachables and extractables of TOPAS COC preserve food and drug stability and quality. It is a non-polar substrate that does not promote adsorption, denaturation, aggregation, or precipitation like glass can. This grade has a high (130°C) heat distortion temperature to withstand 121°C steam sterilization protocols, as well as gamma and EtO procedures.

Key applications and attributes:

  • Drug delivery: Low leachables & extractables, low water transmission
  • Prefilled syringes, vials, cartridges: Non-ionic, does not promote adsorption like glass
  • Bottles: Minimally reactive, EtO/gamma/steam sterilizable
  • Surgical instruments: Chemically resistant to alcohol, acetone, and acrylates
  • IV containers and components: Transparent, withstands EtO/gamma/steam sterilization
  • Labware: Temperature resistance, clarity and purity
  • Optics: Clarity, low birefringence, low moisture sensitivity
  • Electronics: Low dielectric constant, thermoplastic
  • Healthcare and food: Broad regulatory approval

Information provided by Polyplastics USA, which merged with TOPAS Advanced Polymers in 2018.

Key Words: Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Water Absorption at Saturation 0.010 %
@Temperature 23.0 °C
ISO 62
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 63.0 MPa5mm/min; ISO 527-2,-1A
Elongation at Yield 2.6 %5mm/min; ISO 527-2/1A
Tensile Modulus 2900 MPa1mm/min; ISO 527-2/1A
Charpy Impact Unnotched 1.40 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.170 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °CISO 75-1,-2
Glass Transition Temp, Tg 142 °C10°C/min; ISO 11357-1,-2,-3
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.53ISO 489
Transmission, Visible 91 %ISO 13468-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyplastics TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 6013F-04 Cyclic Olefin Copolymer (COC)

POTOPAS08b / 142641

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.