MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

IRPC Polimaxx Polene R1760 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: CHARACTERISTICS: HIGH IMPACT STRENGTH, EXCELLENT SURFACE APPEARANCE, GOOD RIGIDITY CONTAIN UV STABILIZER ADDITIVE

APPLICATIONS: INJECTION MOLDING FOR CRATES, TRAYS, CASES, INDUSTRIAL PARTS, BINS, LARGE HOUSWARES, SAFETY HELMETS PACKAGINGS OF AGRICULTURE PRODUCTS, PALLETS, HEAVY DUTY ARTICLES

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.957 g/cc0.0346 lb/in³ASTM D792
Environmental Stress Crack Resistance >= 9.0 hour>= 9.0 hourCondition B, F50; ASTM D1693
Melt Flow  6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 17.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
17.5 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 65.565.5DIN 53505
Tensile Strength at Break 15.0 MPa2180 psiASTM D638
Tensile Strength, Yield 29.5 MPa4280 psiASTM D638
Elongation at Break 1000 %1000 %ASTM D638
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²DIN 53453
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 125 °C257 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 - 260 °C392 - 500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Global B-8200 High Density Polyethylene
Ipiranga Petrochem HC 7260 HDPE
Ipiranga Petrochem HD 7255 LS-L HDPE
IRPC Polimaxx Polene GA3245 High Density Polyethylene
NIZHNEKAMSKNEFTEKHIM PE 2060S (60105) High Density Polyethylene

PIRPC039 / 84016

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.