MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hapco Hapsil 2021-5 Thermoset
Categories: Polymer; Thermoset

Material Notes: Steralloy™ is a specialty polymer series from Hapco that has been specifically formulated for applications where biocompatibility is required. Prototyping, food processing equipment, medical devices, prosthetics, and filtration are just a few of the applications where Steralloy™ is used.

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D-4669
Viscosity 2500 cPASTM D-4878
Linear Mold Shrinkage 0.0020 - 0.0040 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25ASTM D-2240
Tensile Strength 300 psiASTM D-638
Elongation at Break >= 1200 %ASTM D-638
Izod Impact, Notched NBASTM D-256
Izod Impact, Unnotched NBASTM D-256
Tear Strength 65.0 pliASTM 624 Die C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 4.00 hour
@Thickness 3.17 mm
Demold
Gel Time 5.00 min
@Load 0.100 kg
ASTM D-2971
 
Descriptive Properties
Color (cured)clear / translucent
Mix Ratio100:200Volume
 100:200Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHAPCO147 / 317206

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.