MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Anderol ANDEROL® HTC Chain & Way Fluid, Synthetic Food Grade ISO 220  (discontinued **)
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Description: ANDEROL HTC Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA where incidental food contact can occur. ANDEROL HTC Fluids are recommended for use in chains and ways, including high water applications. They can also be used in lowspeed gear sets, bearings and circulation systems. ANDEROL food grade lubricants are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. ANDEROL food grade lubricants are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.”

Information provided by ConocoPhillips.

Anderol® is a registered trademark of The Anderol Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.860 g/cc0.860 g/ccASTM D-1298
Saybolt Viscosity at 100°F 996 SUS996 SUSASTM D-2161
Saybolt Viscosity at 210°F 106 SUS106 SUSASTM D-2161
Kinematic Viscosity at 40°C (104°F) 220 cSt220 cStASTM D-445
Kinematic Viscosity at 100°C (212°F) 22 cSt22 cStASTM D-445
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 72.6 kg160 lb (mass)ASTM D-2793
 
Thermal PropertiesMetricEnglishComments
Pour Point -35.0 °C-31.0 °FASTM D-97
Flash Point 224 °C435 °FASTM D-92
 
Compliance PropertiesMetricEnglishComments
USDA YesYes
 
Descriptive Properties
Rust TestPassASTM D665A

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON299 / 75336

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.