MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QSil 960 55 Shore A, Condensation Cure for Potting Applications
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QSil 960 is a red, high temperature, self-leveling, two-component, condensation cure, silicone material primarily intended for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section Catalyst by weight which gives a self leveling material with a work life of approximately 60 minutes. The material will be fully cured after 24 – 36 hours at room temperature. The 0.5% catalyst level can be increased or decreased to obtain desired cure speed.

Key Features:

  • Self-leveling
  • Variable cure speed
  • Excellent thermal stability
  • Retention of elastomeric properties within the temperature range of - 115°C – 260°C

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %Uncatalyzed
Viscosity 6500 cPUncatalyzed, Deep Section Catalyst
 24000 cPUncatalyzed, QSil 960
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60Cured 24 hrs at RT
Tensile Strength 500 psiCured 24 hrs at RT
Elongation at Break 130 %Cured 24 hrs at RT
Tear Strength 20.0 pliCured 24 hrs at RT
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+14 ohm-cm
Dielectric Constant 3.9
@Frequency 1000 Hz
Dielectric Strength 21.7 kV/mm
Dissipation Factor 0.020
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
@Temperature 25.0 °C
Gel Time 60.0 min
 
Descriptive Properties
ColorBeigeUncatalyzed, Deep Section Catalyst
 Clear/light yellowUncatalyzed, DBT Catalyst
 RedUncatalyzed, QSil 960
 RedCatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QM 258 60 Shore A, Addition Cure Moldmaking Material
Garlock 502 Silicone Sheet Rubber
3M 7660-S Cold Shrink Silicone Rubber Termination Kits QT-III
Shin-Etsu Silicones LIMS™ KEG2002-60A/B Elastomer
Shin-Etsu Silicones LIMS™ KEG2000-60A/B Elastomer

PACC2110 / 199498

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.