MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Nouryon Levasil CB301 Colloidal silica
Categories: Other Engineering Material

Material Notes: Levasil CB301 is a neutral, aqueous dispersion of colloidal silica that is approximately 28% solids by weight. The silica dispersion is sterically stabilized and the amorphous silica particles carry a negative surface charge. The silica particles are discrete, have a smooth, spherical shape, and are present in a narrow particle size distribution. The particles have also been surface modified with an epoxy silane. The physical appearance of the dispersion is a clear liquid, slightly more viscous than water. Levasil CB301 is produced for world-wide distribution.

CAS number 7631-86-9

Applications: Levasil CB301 is a specialty product primarily used in formulations intended for concrete densification and finishing aid for concrete surfaces. It can also be used as an admixture for concrete.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Particle Size 7.0 µm7.0 µm
pH 8.08.0
Viscosity 5.0 cP5.0 cP
Storage Temperature 0.000 - 40.0 °C32.0 - 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
Content2.5 wt%Ethanol
 28 wt%Silica

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY630 / 286153

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.