MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt Lithobraze 925 Silver Based Cadmium Free Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes:

Applications: The principal use to date of Litho braze 925 has been the brazing of honeycomb panel sections. It can be used for general purpose furnace brazing of stainless steels where flux must be avoided.

Characteristics: Litho braze 925 is lithium modified sterling silver, designed primarily for fluxless furnace brazing of stainless steels. This alloy has been widely used for brazing honeycomb airframe structures made of precipitation hardening stainless steels such as 17-7PH, PH15-7Mo and AM350.

The use of Litho braze 925 permits taking advantage of the maximum panel strength afforded by free node flow. This alloy is not suitable for torch brazing in air but must be used in a hydrogen or inert atmosphere of low dew point (-70EF/-55EC or drier). Argon is the most commonly used inert gas.

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.11 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000312 ohm-cm
@Diameter 0.762 mm
annealed wire with 0.22% Li
 
Thermal PropertiesOriginal ValueComments
Melting Point 1400 - 1635 °F
Solidus 1400 °FMelting Point
Liquidus 1635 °FFlow Point
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu >= 6.55 %
Lithium, Li 0.15 - 0.30 %
Other, total <= 0.15 %
Silver, Ag 92 - 93 %
 
Descriptive Properties
ColorSilver-White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Gold, Au; 18K, White Composition Spec (UNS P00275)
Gold, Au; 18K, Yellow (UNS P00255)
Indium Corp. Indalloy 215 Silver Solder Alloy
Lucas-Milhaupt Cerametil 716 Active Metal Brazing

NLUCMI40 / 18107

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.