MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Covestro Apec® DP9-9340R High-Heat Polycarbonate, Medical with Release  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, High Heat

Material Notes:

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Water Absorption 0.20 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0070 - 0.0080 cm/cmASTM D955
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 330 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 83ASTM D785
Hardness, Rockwell R 127ASTM D785
Tensile Strength, Ultimate 64.0 MPaASTM D638
Tensile Strength, Yield 66.0 MPaASTM D638
Elongation at Break 80 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Tensile Modulus 2.20 GPaASTM D638
Flexural Yield Strength 86.0 MPaASTM D790
Flexural Modulus 2.28 GPaASTM D790
Izod Impact, Notched 3.20 J/cm
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched NBASTM D256
 NB
@Temperature -40.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+16 ohmASTM D257
Dielectric Constant 2.9
@Frequency 60 Hz
ASTM D150
 2.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength >= 16.0 kV/mm
@Thickness 3.17 mm
ASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D150
 0.010
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 162 °C
@Thickness 3.20 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
@Thickness 3.17 mm
ASTM D648
Vicat Softening Point 172 °CRate B; ASTM D1525
Oxygen Index 24 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.578ASTM D542
Haze 1.0 %
@Thickness 3.17 mm
ASTM D1003
Transmission, Visible 88 %
@Thickness 3.20 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 310 - 330 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Hydex™ 202 Rigid Polyurethane (PU)
YOUJU New Materials Paryls® PPSU F1150
YOUJU New Materials Paryls® PPSU F1350 High Flow
Westlake Plastics Zelux® GS Polycarbonate - Gamma Stabilized For Medical Applications
Covestro Baymedix® AP501 Polyurethane

PB1A02 / 26384

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.