MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dover Chemical BASE 12SE Sulfurized Methyl Ester, Lubricity/Extreme Pressure Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Base 12 SE is a sulfurized methyl ester designed to offer both lubricity and extreme pressure properties in oil and water dilutable metalworking fluids. Base 12 SE contains active sulfur and is NOT suitable for products destined for use in yellow metal applications, as it will stain. Base 12 SE can be utilized in straight oil machining, drawing and stamping, as well as a soluble oil component. Base 12 SE may be stored in an original container or bulk storage tank. Prolonged exposure to 0°F may result in solidification. If the product solidifies, warming to 100-110°F will reconstitute the product. Recommended blending temperatures should not exceed 100-130°F.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/cc
@Temperature 25.0 °C
Density 8.10 lb/gal
Saybolt Viscosity at 100°F 110 SUS
Saybolt Viscosity at 210°F 42 SUS
Kinematic Viscosity at 40°C (104°F) 19 cSt
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 4.0[mgKOH/g]
 
Thermal PropertiesOriginal ValueComments
Pour Point 55.0 °F
Flash Point >= 177 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Sulfur, S 2.0 - 4.0 %Active
 13 %Total
 
Descriptive Properties
Copper Corrosion4a10% in oil, 3 hrs, 210°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER100 / 217719

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.