MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
3D Systems LaserForm® Ni718 (A) Nickel Super Alloy, AGED 2
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: A Nickel-based alloy fine-tuned for use with ProX® DMP 320 metal powder, producing parts for high temperature applications. LaserForm Ni718 (A) has outstanding corrosion resistance in various corrosive environments and excellent cryogenic properties. LaserForm Ni718 (A) is formulated specifically for 3D Systems DMP 320 metal 3D Printers to deliver highest part quality and best part properties.

LaserForm Ni718 (A) is a nickel-based heat resistant alloy. This precipitation-hardening nickel-chromium alloy is characterized by good tensile, fatigue, creep and rupture strength at temperatures up to 700°C. Moreover it has outstanding corrosion resistance in various corrosive environments as well as excellent cryogenic properties. These benefits make LaserForm Ni718 (A) ideal for many high temperature applications such as gas turbine parts, instrumentation parts, power and process industry parts etc. Parts can be posthardened to 40 HRC by precipitation-hardening heat treatments. The parts can be machined, spark-eroded, welded, shot-peened, polished and coated if required.

The chemical composition of LaserFormTM Ni718 Type (A) meets the requirements of ASTM F3055-14a.

Information provided by 3D Systems

Key Words: ASTM F3055-14a
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.20 g/ccAbsolute theoretical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 41 - 42ASTM E18
Tensile Strength, Ultimate 1320 - 1360 MPaVertical direction — Z; ASTM E8M
 1370 - 1430 MPaHorizontal direction — XY; ASTM E8M
Tensile Strength, Yield 1180 - 1220 MPaRp0.2%, Vertical direction - Z; ASTM E8M
 1200 - 1260 MPaRp0.2%, Horizontal direction - XY; ASTM E8M
Elongation at Break 12 - 16 %Vertical direction — Z; ASTM E8M
 13 - 17 %Horizontal direction — XY; ASTM E8M
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.2 µm/m-°C
@Temperature 200 °C
 13.9 µm/m-°C
@Temperature 600 °C
Thermal Conductivity 11.4 W/m-K
@Temperature 21.0 °C
 18.3 W/m-K
@Temperature 100 °C
Melting Point 1260 - 1335 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.20 - 0.80 %
Boron, B <= 0.0060 %
Carbon, C <= 0.080 %
Chromium, Cr 17 - 21 %
Cobalt, Co <= 1.0 %
Copper, Cu <= 0.30 %
Iron, Fe 11.147 - 24.6 %Balance
Lead, Pb <= 0.0010 %
Manganese, Mn <= 0.35 %
Molybdenum, Mo 2.8 - 3.3 %
Nb + Ta 4.75 - 5.5 %
Nickel, Ni 50 - 55 %
Phosphorus, P <= 0.015 %
Selenium, Se <= 0.0010 %
Silicon, Si <= 0.35 %
Sulfur, S <= 0.015 %
Titanium, Ti 0.65 - 1.15 %
 
Descriptive Properties
Surface Roughness3-5µmHorizontal direction (XY), AS BUILT
 3-5µmHorizontal direction (XY), AS BUILT
 3-5µmVertical direction (Z), SANDBLASTED
 5-7µmVertical direction (Z), SANDBLASTED

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAPPR3175 / 239143

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.