MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyram RamSter PF701 PBT, UV Stabilized
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: UV stabilized high viscosity PBT for injection molding applications

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³DIN 53479
Water Absorption 0.60 %0.60 %DIN 53495
Moisture Absorption at Equilibrium 0.20 %0.20 %23° C, 50% RH; DIN 53714
Linear Mold Shrinkage 0.021 cm/cm0.021 in/in
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 250 °C
25 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psiASTM-D638
Elongation at Break 60 %60 %ASTM-D638
Flexural Strength 95.0 MPa13800 psiASTM D790
Flexural Modulus 3.00 GPa435 ksiASTM-D790
Izod Impact, Notched 0.500 J/cm
@Temperature 23.0 °C
0.937 ft-lb/in
@Temperature 73.4 °F
ASTM-D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmDIN 53482
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 30.0 kV/mm762 kV/inVDE 0303/4
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FDIN 53461
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Glow Wire Test 750 °C1380 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram RamSter PF713 PBT, UV Stabilized
Polyram RamSter PF702 PBT, UV Stabilized
BASF Ultradur® B 6550 PBT
Celanese Hytrel® DYM250S BK472 TPC-ET+PBT
Covestro Makroblend® DP UT6007 Polycarbonate + PBT, Impact Grade

PPOLYRA156 / 57418

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.