MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Pyrotek Ceramite® AFA Refractory
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Ceramite® AFA Series is a castable refractory material based on fused alumina. Used in demanding applications with extreme temperature requirements, Ceramite AFA’s ceramic bonding provides high strength and good thermal and chemical resistance. Products made from Ceramite AFA are cast into a finished shape and fired prior to delivery. The aggregates in this formulation have a maximum grain size of 6 millimeters (0.24 inches).

Benefits:

  • High maximum service temperature
  • Good strength
  • Moderate thermal conductivity
  • Good chemical resistance

Information provided by Pyrotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  3.10 g/cc
@Temperature 1000 °C
0.112 lb/in³
@Temperature 1830 °F
 3.20 g/cc
@Temperature 20.0 °C
0.116 lb/in³
@Temperature 68.0 °F
Grain Size <= 6000 µm<= 6000 µm
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.00200 GPa
@Temperature 20.0 °C
0.290 ksi
@Temperature 68.0 °F
Cold
 >= 0.0280 GPa
@Temperature 1000 °C
>= 4.06 ksi
@Temperature 1830 °F
Hot
 0.0290 GPa
@Temperature 1000 °C
4.21 ksi
@Temperature 1830 °F
Cold
 0.0320 GPa
@Temperature 1500 °C
4.64 ksi
@Temperature 2730 °F
Cold
 0.0390 GPa
@Temperature 1200 °C
5.66 ksi
@Temperature 2190 °F
Cold
Compressive Strength  0.00900 MPa
@Temperature 20.0 °C
1.31 psi
@Temperature 68.0 °F
Cold
 0.193 MPa
@Temperature 1000 °C
28.0 psi
@Temperature 1830 °F
Cold
 0.200 MPa
@Temperature 1200 °C
29.0 psi
@Temperature 2190 °F
Cold
 >= 0.250 MPa
@Temperature 1500 °C
>= 36.3 psi
@Temperature 2730 °F
Cold
Abrasion  1.1
@Temperature 1000 °C
1.1
@Temperature 1830 °F
[cm^3]
 8.9
@Temperature 20.0 °C
8.9
@Temperature 68.0 °F
[cm^3]
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  3.40 W/m-K
@Temperature 900 °C
23.6 BTU-in/hr-ft²-°F
@Temperature 1650 °F
 3.70 W/m-K
@Temperature 600 °C
25.7 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 4.30 W/m-K
@Temperature 300 °C
29.8 BTU-in/hr-ft²-°F
@Temperature 572 °F
Maximum Service Temperature, Air 1800 °C3270 °F
Shrinkage -0.600 %
@Temperature 20.0 - 850 °C
-0.600 %
@Temperature 68.0 - 1560 °F
 
Descriptive Properties
Permanent Linear Change-0.08%20-850°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Ceramite® CSR Refractory
Pyrotek Ceramite® T-D Dry Sprayable Gunite Refractory
Pyrotek Ceramite® T-W Wet Sprayable Shotcrete Refractory
Pyrotek Ceramite® T Trowellable Refractory

CPYRO501 / 199523

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.