MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Nondezincification Alloy, UNS C99400, Copper Casting Alloy, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Centrifugal Cast

Casting Characteristics: High – Shrinkage in Solidification; Medium - Fluidity, Drossing; Low - Gassing

Fabrication Properties: Excellent Suitability – Soldering, Brazing

Typical uses: Electrical Parts; Gears for Mining Equipment; Propeller Wheels; Valve Stems; Outboard Marine Components

Applicable Specifications: As Sand Cast – Castings ASTM B763/B763M; Ingot - ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.300 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 125
@Load 3000 kg
 170
@Load 3000 kg
Tensile Strength >= 60.0 ksifor Standard
 66.0 ksiTypical
 79.0 ksiTypical
Tensile Strength, Yield >= 30.0 ksifor Standard, 0.5% Ext
 34.0 ksiTypical, 0.5% Ext
 54.0 ksiTypical, 0.5% Ext
Elongation at Break >= 20 %for Standard
 25 %Typical
Tensile Modulus 19300 ksi
Machinability 50 %
Shear Strength 48.0 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000102 ohm-cm16.8% IACS
 
Thermal PropertiesOriginal ValueComments
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 600 °FStress Relief
Solution Temperature 1625 °F
@Time 3600 sec
Water
Precipitation Temperature 900 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.50 - 2.0 %
Copper, Cu 83.9 - 96.5 %As Balance
Iron, Fe 1.0 - 3.0 %
Lead, Pb <= 0.090 %
Manganese, Mn <= 0.50 %
Nickel, Ni 1.0 - 3.5 %
Silicon, Si 0.50 - 2.0 %
Zinc, Zn 0.50 - 5.0 %
 
Descriptive Properties
Proportional Limit29 ksi

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC99400x1 / 293264

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.