MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

UBE 7024B Five Layer Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Specialties:
  • High transparency
  • Good thermoform-ability
  • Low W.V.T.R
  • High shrink-ability
  • Lower extrusion temperature

Processing: Best match for co-extrusion with EVOH resins.

Typical Applications:

  • Cereal packages
  • Flavor barrier (compare with HDPE)
  • Form-fill-seal (Air blown)

Information provided by UBE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Oxygen Transmission Rate 1.00 - 2.00 cc/m²/day0.0644 - 0.129 cc/100 in²/day
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 17.0 MPa2470 psi
Film Tensile Strength at Yield, TD 18.0 MPa2610 psi
Film Elongation at Break, MD 440 %440 %
Film Elongation at Break, TD 480 %480 %
Film Tensile Strength at Break, MD 41.0 MPa5950 psi
Film Tensile Strength at Break, TD 43.0 MPa6240 psi
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 °C410 °FC1
 220 °C428 °FC2
 220 °C428 °FC3
 220 °C428 °FAD
 220 °C428 °FF
 
Descriptive Properties
Layer Structure7024B / Ad / EVOH / Ad/ Surly: (20 / 10 / 20 / 10 / 70 um)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
UBE 7024B Nylon 6/12 Copolymer Film
UBE 5033FDX27 Air Blown Nylon 6/66 Film

PUBE043 / 71603

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.