Petrothene GA1832 resin is a pelletized linear low density polyethylene selected by customers for applications that require maximum strength and toughness. This product offers excellent additive homogeneity, requires no transfer equipment modification, and facilitates clean and safe handling. Typical applications include cast stretch film for pallet utilization. The GA1832 resin offers enhanced film strength, drawdown, toughness, and heat seal strength. Availability: Asia-Pacific; Europe; North America; South & Central America Application: Cast Stretch Film For Pallet Utilization Market: Flexible Packaging Processing Method: Cast Film; Sheet and Profile Extrusion Information provided by LyondellBasell. |