MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Dow AFFINITY™ PL 1850 Polyolefin Plastomer
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE

Material Notes: AFFINITY® PL 1850 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown and cast film products with low temperature sealability, excellent optics and good abuse resistance. It finds applications as a sealant layer in multilayer film structures for dry and liquid packaging. AFFINITY PL 1850 has excellent compatibility with other polyolefins, allowing efficient blending and coextrusion. It complies with FDA regulation 21 CFR 177.1520c3.1b, which allows for its use in direct food contact applications.

Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³
Thickness 25.0 microns0.984 mil
Melt Flow 3.0 g/10 min
@Load 2.16 kg
3.0 g/10 min
@Load 4.76 lb
Melt flow ratio I10/I2 is 8.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 5.70 MPa827 psi
Film Tensile Strength at Yield, TD 4.80 MPa696 psi
Film Elongation at Break, MD 440 %440 %
Film Elongation at Break, TD 720 %720 %
Secant Modulus, MD 0.0690 GPa10.0 ksiFilm value
Secant Modulus, TD 0.0712 GPa10.3 ksiFilm value
Elmendorf Tear Strength MD 300 g300 g
Elmendorf Tear Strength TD 480 g480 g
Elmendorf Tear Strength, MD 12.0 g/micron305 g/mil
Elmendorf Tear Strength, TD 19.2 g/micron488 g/mil
Dart Drop >= 33.2 g/micron>= 843 g/mil
Film Tensile Strength at Break, MD 41.5 MPa6020 psi
Film Tensile Strength at Break, TD 46.1 MPa6690 psi
 
Optical PropertiesMetricEnglishComments
Haze 0.40 %0.40 %
Gloss 95 %95 %45°
 
Processing PropertiesMetricEnglishComments
Processing Temperature 94.0 °C201 °FSeal initiation temperature
 274 °C525 °FFilm extrusion temperature
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AFFINITY™ PL 1845 Polyolefin Plastomer
Dow AFFINITY™ KC 8852 Polyolefin Elastomer
Dow AFFINITY™ EG 8150 Polyolefin Elastomer
Dow AFFINITY™ PL 1840 Polyolefin Plastomer
Dow AFFINITY™ FM 1570 Polyolefin Plastomer

PDW405 / 34474

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.