MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Miracll C85 Polycarbonate-based TPU, C Series
Categories: Polymer; Thermoplastic; Polyurethane, TP; Polycarbonate-Urethane

Material Notes: Excellent aging resistance, oil resistance, hydrolysis resistance, high temperature resistance, UV resistance, excellent physical properties & weathering resistance, etc. Applications: hose & tube, film & sheet, fire hose, oil tank.

Information provided by Miracll Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 86ASTM D2240
Tensile Strength 40.0 MPaASTM D412
Elongation at Break 450 %ASTM D412
100% Modulus 0.00700 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0160 GPa
@Strain 300 %
ASTM D412
Tear Strength 100 kN/mASTM D624
Abrasion 25DIN Abrasion Loss; DIN 53516
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -25.0 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Pellethane® 2363-90AE TPU
Lubrizol LifeSciences Carbothane® AC-4085A-B20 Aromatic TPU
Lubrizol LifeSciences Carbothane® AC-4085A TPU – Clear Aromatic
Lubrizol Estane® S190A Thermoplastic Polyurethane
Lubrizol Estane® S185A Thermoplastic Polyurethane

PMIRAC81 / 221410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.