MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Elastosil® R plus 4001/40 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product description: HCR silicone rubbers of the ELASTOSIL® R plus 4001 series are addition-curing, one-component compounds for the manufacture of press cured articles. The vulcanizates show excellent transparency and good to very good mechanical properties. No peroxide split products are released during cure or post cure. Cure system is significantly faster compared to peroxide curing materials. Properly postcured vulcanizates of ELASTOSIL® R plus 4001 comply with BfR and FDA food contact regulations. Cure time is reduced to 30 - 50 % depending on the wall thickness.

Special features:

  • easy demolding
  • dry surface
  • no unpleasant smell caused by peroxides
  • no inhibition by oxygen
Application: The grade is suitable for the manufacture of all kind of articles for technical and food-contact applications. Specially thick walled articles can take advantage of the fast curing material.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183-1 A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40DIN 53505
Tensile Strength at Break 11.5 MPaDIN 53504 S1
Elongation at Break 750 %DIN 53504 S1
Rebound 57 %DIN 53512
Tear Strength 35.0 kN/mASTM D624 B
Compression Set 20 %
@Temperature 175 °C,
Time 79200 sec
DIN ISO 815-B
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Treatment Temp. 165 °C
post cured 4h/200°C
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9265 / 204794

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.