MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Surpass® FPs236-A Octene sMDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Film Grade

Material Notes: FPs236-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPs236-A is subject to the specific limitation that it may contact food only at temperatures of 212°F and below.

NOVA Chemicals' polyethylene resins are biologically and chemically inert.

Features: Excellent tensile and elongation properties, Good optical properties, Low gel level

Additives: High temperature AO

Applications: Cast film, Co-extrusion and lamination

Film properties are typical of cast film extruded at a melt temperature of 500°F, and a line speed of 600 ft/min.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.936 g/ccASTM D 792
Thickness 25.0 micronsAs tested for properties on this data sheet
Melt Flow 2.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 14.2 MPaASTM D 882
Film Tensile Strength at Yield, TD 15.1 MPaASTM D 882
Film Elongation at Break, MD 600 %ASTM D 882
Film Elongation at Break, TD 900 %ASTM D 882
Elmendorf Tear Strength MD 40 gASTM D 1922
Elmendorf Tear Strength TD 350 gASTM D 1922
Elmendorf Tear Strength, MD 1.60 g/micronASTM D 1922
Elmendorf Tear Strength, TD 14.0 g/micronASTM D 1922
Dart Drop 1.60 g/micronASTM D 1709/A
Dart Drop Test 40.0 gF50; ASTM D 1709/A
Film Tensile Strength at Break, MD 45.0 MPaASTM D 882
Film Tensile Strength at Break, TD 35.0 MPaASTM D 882
1% Secant Modulus, MD 300 MPaASTM D 882
1% Secant Modulus, TD 370 MPaASTM D 882
 
Optical PropertiesOriginal ValueComments
Haze 4.8 %ASTM D 1003
Gloss 80 %At 45°; ASTM D 2457
 
Descriptive Properties
Low Friction Puncture24 (J/mm)NOVA Chemicals test method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 75 Micron Film
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin

PNOV775 / 108900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.