MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MRC Polymers NAXELL™ PC110-919 General Purpose Polycarbonate, Medium High MFR
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes:
  • Polycarbonate for colorable products
  • MFR can be modified between 10 to 40 g/10min
  • Can be UV stabilized
  • Internal and external lubricant can be added
  • Can be clear to color matched
  • Not for products that require stringent visual specification
  • FR package can be added

Information provided by MRC Polymers Inc.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccsolid; ASTM D792
Water Absorption 0.15 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/in
@Thickness 3.17 mm
ASTM D955
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
nominal; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 9000 psi
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D638
Elongation at Break 60 %
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D638
Flexural Strength 14.0 ksi
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D790
Flexural Modulus 340 ksi
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D790
Izod Impact, Notched 16.0 ft-lb/in
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D256
Dart Drop, Total Energy 45.0 ft-lb
@Thickness 3.17 mm,
Temperature 22.8 °C
7.5MPH; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µm/m-°C
@Temperature -40.0 - 35.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 275 °F
@Thickness 3.17 mm
un-annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 257 °F
@Thickness 3.17 mm
un-annealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 490 - 520 °F
Middle Barrel Temperature 510 - 540 °F
Front Barrel Temperature 530 - 560 °F
Nozzle Temperature 530 - 560 °F
Melt Temperature 520 - 560 °F
Mold Temperature 120 - 200 °F
Drying Temperature 240 °F
Dry Time 3 - 4 hour
Moisture Content <= 0.020 %
Dew Point <= 0.000 °F
Drying Air Flow Rate 0.800 - 1.00 ft³/min (CFM)per lb/hour resin processed
Injection Pressure 10000 - 20000 psi
Back Pressure 50.0 - 175 psi
Cushion 0.250 in
Screw Speed 50 - 75 rpm
 
Descriptive Properties
Fill RateModerate
Hold Pressure40-60% of injection pressure
Packing Pressure50-75% of injection pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 301 HMR FC030003 Polycarbonate Resin
Chi Mei Wonderlite® PC-110 Polycarbonate
Avient Edgetek® PC-40GF-000 FR MR Polycarbonate (PC), Glass Filled
MRC Polymers NAXELL PC100H High MFR Polycarbonate
Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable

PMRC030 / 89459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.