MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Corning Polarcor™ WIDE Band™ Glass Polarizer, 600 - 1100 nm Nominal Wavelength
Categories: Ceramic; Glass; Optical

Material Notes: Polarcor™ is used as an optical element in polarization-dependent isolators, optical modulators, polarimetry systems, ellipsometers, shutters and other polarization-based devices. Polarcor is characterized by high extinction and low insertion loss throughout the 600 nm to 2300 nm wavelengths (depending on grade). Polarcor is a borosilicate glass that contains titanium, aluminum and silver. The polarizing mechanism is elongated silver crystals in the outer 20 µm ? 50 µm of the glass surface; this ensures the elimination of stray light, by absorbing the unwanted polarization. Since Polarcor is a solid glass product it is extremely resistant to chemical, physical and thermal damage, while exhibiting excellent optical properties.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.412 g/cc0.08714 lb/in³
Thickness 500 microns19.7 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 480480kg/mm2
Modulus of Elasticity 58.6 GPa8500 ksi
Poissons Ratio 0.210.21
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.50 µm/m-°C3.61 µin/in-°F
Specific Heat Capacity 0.770 J/g-°C0.184 BTU/lb-°Festimated by Corning
Thermal Conductivity  1.00 W/m-K
@Temperature 1.00 °C
6.96 BTU-in/hr-ft²-°F
@Temperature 33.8 °F
 1.13 W/m-K
@Temperature 100 °C
7.83 BTU-in/hr-ft²-°F
@Temperature 212 °F
 1.26 W/m-K
@Temperature 200 °C
8.70 BTU-in/hr-ft²-°F
@Temperature 392 °F
 1.38 W/m-K
@Temperature 300 °C
9.57 BTU-in/hr-ft²-°F
@Temperature 572 °F
 1.46 W/m-K
@Temperature 400 °C
10.1 BTU-in/hr-ft²-°F
@Temperature 752 °F
 1.59 W/m-K
@Temperature 500 °C
11.0 BTU-in/hr-ft²-°F
@Temperature 932 °F
 1.80 W/m-K
@Temperature 600 °C
12.5 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5107 - 1.5218
@Wavelength 600 - 1100 nm
1.5107 - 1.5218
@Wavelength 600 - 1100 nm
Abbe Number 57.657.6
Transmission, Visible  >= 60 %
@Wavelength 600 - 1100 nm
>= 60 %
@Wavelength 600 - 1100 nm
Insertion Loss without AR-Coating < 2.2 dB
 >= 66 %
@Wavelength 600 - 1100 nm
>= 66 %
@Wavelength 600 - 1100 nm
Insertion Loss for 2 sides AR-Coated < 1.8 dB
Reflection Coefficient, Visible (0-1) <= 0.010<= 0.010Reflectance R per each side
 
Descriptive Properties
Brewster's Angle56.3°
Contrast>10,000:1Extinction Ration > 40 dB
Polarization Bandwidth (nm)600 - 1100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CCORNG928 / 282899

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.