MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cabot BLACK PEARLSĀ® 717 Specialty carbon black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: BLACK PEARLS 717 specialty carbon black delivers an attractive balance of medium jetness, deep blue undertone, easy processing, and good surface quality for coloration of plastic molded parts. It can enable excellent aesthetic performance for moldings used in numerous visible applications.

Key applications: BLACK PEARLS 717 specialty carbon black is used in a variety of applications that require aesthetic performance in plastic molded parts. Its blue undertone makes it a good choice when designers require bluish tones and do not require the level of jetness provided by BLACK PEARLS 800 specialty carbon black products. Its dispersibility assists molders in achieving good surface quality. Additionally, it can typically be loaded into masterbatches at higher dosages than other carbon blacks used for similar applications while still maintaining good masterbatch dilutability. It is typically used for visible parts in:

  • Appliances
  • Sport, leisure, and toy products
  • Housewares
  • Packaging and containers with demanding requirements
  • Some automotive and electronics applications
BLACK PEARLS 717 specialty carbon black can be used in resins for aesthetic applications including ABS and other styrenics, PC and PC blends, PP, PE, and TPOs. BLACK PEARLS 717 specialty carbon black is a pelletized product. A non-pelletized carbon black having similar morphology is available in an easier-to-disperse fluffy form as MONARCH 717 specialty carbon black.

Performance features:

  • Medium jetness
  • Deep blue undertone
  • Easy processing
  • Imparts good surface quality

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.495 g/ccASTM D-1513
Particle Mesh Size 325 Mesh<200 ppm; ASTM D-1514
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 3.0 %ASTM D-1509
 
Descriptive Properties
Iodine absorption183 mg/gASTM D-1510
OAN55 cc/100gASTM D-2414
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT034 / 315769

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.