Product Description: TINMATE 201 LS Organotin stabilizer is highly effective liquid PVC stabilizer, especially designed for thermally stabilizing Vinyl copolymers, that provides good early color control and long term stability facilitating excellent transparency and color hold with superior processing stability. TINMATE 201 LS - Organotin (Methyl Tin Mercaptide) - PVC Heat Stabilizer is an FDA Approved material under 21 FR 178.2010 for FOOD & Drug contact additives (Plasticizers & Stabilizers) for PVC Applications" Characteristics & Usages: TINMATE is recommended particularly For PVC formulations such as Transparent / Food Grade Rigid & Soft Packaging Films / Sheets and Blow Molded Bottles / Jars & Injection Molded/ Extruded PVC & CPVC Products & components. - Excellent early color & color hold.
- Outstanding Long term dynamic stability
- Sparkling clarity (transparency)
Information provided by Vikas Ecotech LTD |