MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Southern Polymer PRIMALENE® WPP692M LLDPE
Material Notes: A metallocene linear low density polyethylene

Typical Applications:

  • Seal layer in co-extrusions
  • Heavy duty packaging
  • Clarity packaging
Features:
  • High clarity
  • Excellent gloss
  • Excellent toughness
  • Good sealability
  • Processing aid
  • Slip: zero
  • Anti-block: zero

Information provided by Southern Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.7 MPa1550 psiASTM D882
Film Tensile Strength at Yield, TD 9.51 MPa1380 psiASTM D882
Film Elongation at Break, MD 450 %450 %ASTM D882
Film Elongation at Break, TD 600 %600 %ASTM D882
Coefficient of Friction >= 1.0>= 1.0ASTM D1894
Elmendorf Tear Strength, MD 9.06 g/micron230 g/milASTM D1922
Elmendorf Tear Strength, TD 19.7 g/micron500 g/milASTM D1922
Dart Drop 31.5 g/micron800 g/milASTM D1709
Film Tensile Strength at Break, MD 58.6 MPa8500 psiASTM D882
Film Tensile Strength at Break, TD 51.7 MPa7500 psiASTM D882
1% Secant Modulus, MD 175 MPa25400 psiASTM D882
1% Secant Modulus, TD 191 MPa27700 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %4.0 %ASTM D1003
Gloss 130 %130 %60°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOUTH056 / 283912

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.