MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Entec Hylox® 9230BK PBT, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.

Information provided by Entec.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 17000 psiASTM D638
Flexural Strength 24500 psiASTM D790
Flexural Modulus 1.23e+6 psiASTM D790
Izod Impact, Notched 1.49 ft-lb/in73°F; ASTM D256
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 450 - 470 °F
Middle Barrel Temperature 460 - 480 °F
Front Barrel Temperature 470 - 490 °F
Nozzle Temperature 470 - 490 °F
Melt Temperature 480 - 500 °F
Mold Temperature 180 - 250 °F
Drying Temperature 250 °F
Dry Time <= 12 hour
Moisture Content <= 0.020 %
Injection Pressure 1000 - 1700 psi
Back Pressure 20.0 - 60.0 psi
Shot Size 40 - 80 %
Screw Speed 40 - 80 rpm
 
Descriptive Properties
Holding Pressure500 to 900 psi
Injection RateModerate-Fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Entec Hylox® 9030 PBT, 30% Glass Reinforced
Avient Bergadur™ PB40 G30 UF UV Polybutylene Terephthalate (PBT)
Overview of materials for Polycarbonate, Glass + PTFE Filled
Evonik Vestodur® CL2030 30% Glass Reinforced, Crosslinkable PBT Based Compound
Envalior Pocan® B 4235 Z 000000 PBT, 30% Glass Fiber Reinforced

PENT208 / 36248

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.