MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChenGuang TL-160 Low M.W. PTFE Micropowder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: TL-160 is low molecular weight PTFE micropowder. Its particles are with ideal spherical shape and narrow size distribution.Compared to other ordinary PTFE micropowders, TL-160 has superior properties of excellent dispersing performance, large specific surface area, low bulk density, high oil absorption, and low viscosity of its composites with solvents.

Applications: TL-160 is a solid lubricant, usually used as an additive to other materials. Added into plastics or rubbers at 3% - 20%, it can reduce friction cofficient and improve abrasion resistance of the products ; other host materials, such as inks, greases, lubricant oils or coatings, can also benefit from the additive of TL-160 at 0.25% - 10% with lower friction, higher service temperature and prolonged service life. It can also be used for static spray coating as an additive to some organic solvents. Note: Because of its inherent characteristics, TL-160 is not for molding or extrusion applications.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.350 - 0.420 g/cc0.0126 - 0.0152 lb/in³
Particle Size <= 10 µm<= 10 µm
 
Descriptive Properties
Colorwhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU031 / 255630

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.