MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
J6 Polymers JFOAM™ BX-190 Engineered Specialty Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: JFOAM™ BX-190-R is the resin component of a two part polyurethane system, which when combined with the T component, Isocyanate, will produce a water-blown rigid polyurethane foam system. BX-190 issued for void fill and core material applications and can meet some military specifications.

Information provided by J6 Polymers LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccR Component, Polyol Blend
 1.24 g/ccT Component, Polymeric MDI
 1.96 lb/ft³Cup density, #10
 2.40 lb/ft³Core; ASTM D1622
Water Absorption 11.63 %ASTM D2842
Viscosity 200 cPT Component, Polymeric MDI
 1500 cPR Component, Polyol Blend
Storage Temperature 65.0 - 85.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 472 psiParallel; ASTM D1623
 3083 psiModulus; ASTM D1623
Tensile Modulus 41.7 psi
@Temperature 71.1 °C
Parallel; ASTM D1623
 2116 psi
@Temperature 71.1 °C
Modulus; ASTM D1623
Compressive Strength 24.6 psi
@Temperature 71.1 °C
Parallel, 10% deflection; ASTM D1621
 44.5 psi
@Temperature 25.0 °C
Parallel, 10% deflection; ASTM D1621
 583 psi
@Temperature 71.1 °C
Modulus, 10% deflection; ASTM D1621
 960 psi
@Temperature 25.0 °C
Modulus, 10% deflection; ASTM D1621
Shear Modulus 1.026 ksiASTM C723
Shear Strength 24.5 psiASTM C723
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.170 BTU-in/hr-ft²-°FK-Factor; ASTM C518
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Dimensional Stability+0.8% Change1 day, 70°C at 100% RH, ASTM D2126
 -0.16% Change1 day, -29°C, ASTM D2126
 -0.96% Change7 days, -29°C, ASTM D2126
 -1.32% Change14 days, 93.3°C, ASTM D2126
 -1.39% Change7 days, 93.3°C, ASTM D2126
 -1.39% Change7 days, 70°C at 100% RH, ASTM D2126
 -1.45% Change1 day, 93.3°C, ASTM D2126
 -1.53% Change14 days, 70°C at 100% RH, ASTM D2126
 -1.56% Change14 days, -29°C, ASTM D2126
Friability0.1337ASTM C421
Hand Mix Reactivity21 secCream Time
Mixing Ratio0.3R Component, Polyol Blend
 0.7T Component, Polymeric MDI

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
J6 Polymers JFOAM™ A-204 Engineered Specialty Foam
3M RPF-C (0.32 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
3M RPF-C (0.24 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
General Plastics LAST-A-FOAM® R-9320 Thermal Isolation Blocks
General Plastics LAST-A-FOAM® TR-20 Polyurethane Foam

PJSIX007 / 190934

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.