MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Kanthal Nifethal 42 Resistance heating wire and resistance wire
Categories: Metal; Ferrous Metal; Superalloy; Nickel Base

Material Notes: Nifethal 42 is a nickel-iron alloy (NiFe alloy) for use at temperatures up to 600°C (1110°F). The alloys has a moderate constant thermal expansion factor up to 300°C(570°F). Typical applications for Nifethal 42 are in high temperature thermostats in, for example, gas and electric stoves.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.12 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 700 MPa
@Thickness 5.80 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000630 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 15.0 W/m-K
@Temperature 100 °C
Melting Point 1425 °C
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe <= 58 %
Nickel, Ni >= 42 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Assab Steels QRO 90 SUPREME Hot Work Steel
Aperam Invar® FeNi336 Cold Rolled Strip
Alliance N-33 Neodymium Iron Boron Magnetic Material
Hogen HM3750 Tungsten-Based Metal
Hogen Diemitech™ Tungsten-Based Metal

NSANDV5003 / 199567

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.