MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik TROGAMID® myCX Polyamide
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Transparent polyamides are broadly established in the technically demanding fields of automotive, electronics and constructions. The TROGAMID® CX family combines the transparency and processing behavior of amorphous materials with the advantages of polyamides like toughness, rigidity, abrasion resistance, and chemical and stress cracking resistance. When special aliphatic and cycloaliphatic monomers are used, transparent polyamides can be made that have inherently better UV resistance, like TROGAMID® CX9704. In addition, carefully selected monomers yield a crystallizable polyamide, such as TROGAMID® myCX, a PA PACM 12. The crystallites are so small that they don’t scatter visible light. This makes the material appear transparent to the human eye—a property known as microcrystallinity. TROGAMID® CX9704 is the perfect choice for the manufacturing of spectacle frames. It makes possible:
  • freedom of design in shape and color
  • ultra thin frame constructions
  • light weight eyeglass frames
  • durability, robustness and flexibility
In contrast to other transparent amorphous materials, the microcrystalline TROGAMID® myCX demonstrates excellent stress-cracking resistance. It is an unparalleled transparent material that combines the properties of a semi-crystalline molding compound with those of amorphous materials. For lenses that satisfy the most demanding customer, TROGAMID® myCX is preferred because it:
  • provides the highest comfort due to its very low weight
  • offers excellent optical properties
  • delivers the highest safety level possible in sunglass lenses
  • can be combined with all potential
  • frame materials
  • assures highest durability in top quality sunglasses
  • prevents crack formation by stress or chemical attack

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Water Absorption at Saturation 3.5 %ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81ISO 868
Tensile Strength, Yield 60.0 MPaISO 527-1/2
Elongation at Break >= 50 %ISO 527-1/2
Elongation at Yield 8.0 %ISO 527-1/2
Tensile Modulus 1400 MPaISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature 0.000 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 12.0 kJ/m²
@Temperature 0.000 °C
ISO 179/1eA
 14.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°CISO 11359
CTE, linear, Transverse to Flow 90.0 µm/m-°CISO 11359
Deflection Temperature at 1.8 MPa (264 psi) 105 °CISO 75-1/-2
Glass Transition Temp, Tg 140 °CISO 11357
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.513
@Wavelength 656 nm
DIN 53491
 1.516
@Wavelength 489 nm
DIN 53491
 1.523
@Wavelength 488 nm
DIN 53491
Transmission, Visible 91.7 %
@Thickness 2.00 mm
ISO 13468-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Trogamid® A4000 Transparent Polyamide
EMS-Grivory Grilamid® TR XE 4010 PA*-I
Evonik Trogamid® T-GF35 35% Glass Reinforced Amorphous Nylon
Evonik Trogamid® TX7389 Nylon 6-3 Compound
Evonik Trogamid® BX9723 30% Glass Fiber Reinforced Polyamide

PEVONIL200 / 196404

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.