MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Solvay DAPCO™ 3041FR Paste Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: DAPCO™ 3041FR paste adhesive is a two-part, room temperature curing, epoxy-based, 100% solids, self-extinguishing general purpose adhesive. The material has a convenient one-to-one mix ratio by volume. The product is available in a variety of kit sizes including 50 ml, 200 ml and 400 ml side-by-side cartridges, pints, quarts and gallons.

Features & Benefits:

  • Semi-thixotropic flow properties
  • 100% solids content
  • Room temperature cure
  • Room temperature storage
  • 180°F (82°C) performance
  • Meets FAR 25.853
  • One-to-one mix ratio by volume
  • Bonds to a variety of metallic and non-metallic substrates including aramid fibers, acrylic/PVC alloys and polycarbonates such as Kevlar®, Kydex® and Lexan®

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³Part B
 1.10 g/cc0.0397 lb/in³Mixed
 1.15 g/cc0.0415 lb/in³Part A
Solids Content 100 %100 %Mixed
 100 %100 %Part B
 100 %100 %Part A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70 - 8070 - 80ASTM D224
Tensile Strength 34.5 MPa5000 psi
Elongation at Break 10 %10 %
Compressive Strength 42.7 MPa6200 psi
Compressive Modulus 200 GPa29000 ksi
Adhesive Bond Strength  5.52 MPa
@Temperature 82.0 °C
800 psi
@Temperature 180 °F
Shear to Aluminum (2024 T3)
 6.89 MPa
@Temperature 66.0 °C
1000 psi
@Temperature 151 °F
Shear to Aluminum (2024 T3)
 26.2 MPa
@Temperature 25.0 °C
3800 psi
@Temperature 77.0 °F
Shear to Aluminum (2024 T3)
 26.9 MPa
@Temperature -55.0 °C
3900 psi
@Temperature -67.0 °F
Shear to Aluminum (2024 T3)
Peel Strength 3.86 kN/m22.0 pliT-Peel; ASTM D1876
 5.61 kN/m32.0 pliDrum; ASTM D1876
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthPart B
 12.0 Month12.0 MonthPart A
 
Descriptive Properties
ColorAmberPart B
 TanMixed
 WhitePart A
Insert pull-out strength350 psiNAS 1836-7
 700 psiNAS 1836-14
 975 psiNAS 1836-22
Mix Ratio1:1Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elantas EN-2523 (Conap) Potting and Encapsulation Adhesive
Solvay BR® 680-3 Polyimide Film Adhesive
Solvay A6000 ETFE Fluoropolymer Film
Rogers Arlon R35366X020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Parker Chomerics Tecknit Teckfip™ FIP-E Formed in Place Conductive Elastomer

PCYTED020 / 180322

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.