MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Borealis Daplen EH119HP Polypropylene, Mineral Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Daplen EH119HP is a mineral filled elastomer modified polypropylene compound intended for injection molding.

Special Features:

  • Excellent surface appearance
  • Available with and without UV-stabilization
  • High flowability
Applications: EH119HP has been developed especially for the car industry to be used in automotive exterior parts.
  • Bumpers
  • Exterior trims
  • Front grills

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³ISO 1183
Melt Flow 33.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
33.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 17.0 MPa2470 psi50 mm/min; ISO 527-2
Flexural Modulus 1.45 GPa210 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  5.50 kJ/m²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 35.0 kJ/m²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
37.2 µin/in-°F
@Temperature -22.0 - 176 °F
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °C117 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 - 80.0 °C104 - 176 °F
 220 - 260 °C428 - 500 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psi
 
Descriptive Properties
Flow front speed100 - 200 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9681 / 323038

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.