MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SKYi Composites Stabil ML3166 PA66 40 LFT
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: Stabil ML3166 is a special Light and Heat stabilized, long glass fibre reinforced polyamide grade, for injection moulding and extrusion. The long glass fibres, chemically coupled to the polyamide matrix, providing outstanding mechanical properties. Stabil ML3166 is available both in black and natural. Other colours can be provided on request.

Applications: Stabil ML3166 is intended for injection moulding of highly demanding technical applications. The excellent properties of Stabil ML3166 make it suitable for: Electrical components, automotive parts, interior, exterior and under the bonnet, structural furniture parts, load bearing, demanding components for various engineering sectors. Stabil ML3166 can, in many of these applications, substitute other engineering plastics or metal alloys.

Information provided by SKYi

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/cc
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 235 MPa34100 psiISO 527-I
Elongation at Break 2.2 %2.2 %ISO 527-I
Tensile Modulus 16.0 GPa2320 ksiISO 527-I
Flexural Strength 345 MPa50000 psiISO 178
Flexural Modulus 14.0 GPa2030 ksiISO 178
Charpy Impact, Notched 3.30 J/cm²15.7 ft-lb/in²ISO 179-I
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) >= 255 °C>= 491 °FISO 75-I
 
Processing PropertiesMetricEnglishComments
Feed Temperature 275 - 285 °C527 - 545 °F
Nozzle Temperature 285 - 295 °C545 - 563 °F
Melt Temperature 285 - 300 °C545 - 572 °F
Mold Temperature 90.0 - 120 °C194 - 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSKYI008 / 256126

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.