MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Nouryon Butanox P-50 Methyl isopropyl ketone peroxide
Categories: Other Engineering Material

Material Notes: Butanox P-50 is a high-reactive methyl isopropyl ketone peroxide (MIPKP) for the optimal cure of unsaturated polyester resins in the presence of a cobalt accelerator at room and elevated temperatures. Provides less shrinkage and improved exterior quality of the gelcoat.

CAS number: 33373-82-7, 13921-99-8

EINECS/ELINCS No.: 442-480-8

Applications: Butanox P-50 is a high reactive methyl isopropyl ketone peroxide (MIPKP) for the optimal curing of unsaturated polyester resins in the presence of a cobalt accelerator at room and elevated temperatures. The curing system Butanox P-50/cobalt accelerator is particularly suitable for the curing of gelcoat resins and laminating resins used for the production of boat hulls, deck parts, truck panels, car panels or sanitary ware products. Practical experience has proven that by the guaranteed low water content and the absence of polar compounds in Butanox P-50, this peroxide is very suitable in GRP products for high demanding end-markets like marine applications (boat building).

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.1569 g/cc0.041796 lb/in³
Viscosity 20 cP20 cP
Storage Temperature -10.0 - 25.0 °C14.0 - 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 50.0 °C122 °FSelf-Accelerating Decomposition Temperature
 
Descriptive Properties
AppearanceClear colorless liquid
Content6.3-6.5 %Total active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY453 / 285976

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.