MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Features: USP Class VI

Available in Americas, Europe, Middle East, Africa, India and Asia

AvailableInformation provided by Lubrizol

Lubrizol acquired the Isoplast product line from Dow in 2009.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.71 g/ccASTM D792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 33000 psiASTM D638
Tensile Strength, Yield 33000 psiASTM D638
Elongation at Break 2.0 %ASTM D638
Elongation at Yield 2.0 %ASTM D638
Tensile Modulus 2.50e+6 psiASTM D638
Flexural Strength 57000 psiASTM D790
Flexural Modulus 2.20e+6 psiASTM D790
Izod Impact, Notched 16.0 ft-lb/in
@Thickness 3.17 mm,
Temperature -40.0 °C
ASTM D256
 16.0 ft-lb/in
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D256
Dart Drop, Total Energy 25.0 J
@Temperature -28.9 °C
ASTM D3763
 29.0 J
@Temperature 22.8 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 260 °Funannealed; ASTM D648
 260 °Fannealed; ASTM D648
Vicat Softening Point 366 °FASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 238 - 260 °C
Mold Temperature 66.0 - 88.0 °C
Drying Temperature 82.0 - 99.0 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® GV-4H PA*-GF40
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin
Celanese Celstran® TPU-CF40-01 TPU, 40% Specialty
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane
EMS-Grivory Grivory® GV-6H PA*-GF60

PDOW1394a / 138110

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.