MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nimonic 942 Nickel Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.19 g/cc0.296 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  900 MPa
@Temperature 760 °C
131000 psi
@Temperature 1400 °F
Bar
 1240 MPa
@Temperature 650 °C
180000 psi
@Temperature 1200 °F
Bar
 1300 MPa
@Temperature 540 °C
189000 psi
@Temperature 1000 °F
Bar
 1405 MPa
@Temperature 21.0 °C
203800 psi
@Temperature 69.8 °F
Bar
Tensile Strength, Yield  860 MPa
@Strain 0.2 %,
Temperature 760 °C
125000 psi
@Strain 0.2 %,
Temperature 1400 °F
Bar
 970 MPa
@Strain 0.2 %,
Temperature 540 °C
141000 psi
@Strain 0.2 %,
Temperature 1000 °F
Bar
 1000 MPa
@Strain 0.2 %,
Temperature 650 °C
145000 psi
@Strain 0.2 %,
Temperature 1200 °F
Bar
 1060 MPa
@Strain 0.2 %,
Temperature 21.0 °C
154000 psi
@Strain 0.2 %,
Temperature 69.8 °F
Bar
Rupture Strength  270 MPa
@Temperature 760 °C,
Time 3.60e+6 sec
39200 psi
@Temperature 1400 °F,
Time 1000 hour
Bar
 520 MPa
@Temperature 650 °C,
Time 3.60e+6 sec
75400 psi
@Temperature 1200 °F,
Time 1000 hour
Bar
Modulus of Elasticity  157 GPa
@Temperature 650 °C
22800 ksi
@Temperature 1200 °F
 166 GPa
@Temperature 540 °C
24100 ksi
@Temperature 1000 °F
 196 GPa
@Temperature 21.0 °C
28400 ksi
@Temperature 69.8 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.7 µm/m-°C
@Temperature 538 °C
8.17 µin/in-°F
@Temperature 1000 °F
 16.5 µm/m-°C
@Temperature 871 °C
9.17 µin/in-°F
@Temperature 1600 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Melting Point 1240 - 1300 °C2260 - 2370 °F
Solidus 1240 °C2260 °F
Liquidus 1300 °C2370 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.60 %0.60 %
Boron, B 0.010 %0.010 %
Carbon, C 0.030 %0.030 %
Chromium, Cr 12.5 %12.5 %
Iron, Fe 37 %37 %
Manganese, Mn 0.20 %0.20 %
Molybdenum, Mo 6.0 %6.0 %
Nickel, Ni 39.7 %39.7 %as balance
Silicon, Si 0.30 %0.30 %
Titanium, Ti 3.7 %3.7 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nimonic PK25 Superalloy
MetalTek WASPALOY® Centri-Vac Nickel Cobalt Based Alloy
Haynes Waspaloy™ alloy, sheet
ATI Allvac® WASPALOY® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
Special Metals NIMONIC® Alloy 105

NZ983 / 170612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.