MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Selenis AKOLYT KM 900 Copolyester for Film Extrusion
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: Selenis Akolyt KM 900 copolyester has been specifically developed for the extrusion of technical films for furniture lamination, graphics arts, and the card film industry. Films made from Selenis Akolyt KM 900 allow excellent decorative capability, permitting unlimited design freedom and full personalization of the final application. Selenis Akolyt KM 900 grade allows variety of finishes to films, such as embossing techniques and glossy or leather-like surfaces. The exceptional clarity of films produced from Selenis Akolyt KM 900 allow reverse printing technique, enhancing printing optics whilst maximizing artwork protection. Elongation of films produced from Selenis Akolyt KM 900 permit thermoformed deep drawing, at the same time as its relatively low Tg grants energy cost savings while guaranteeing perfect adhesion to the substrates. Proven chemical resistance against common household detergents makes Selenis Akolyt KM 900 the perfect choice for films that will resist everyday weathering.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.730 g/cc
Density >= 1.27 g/ccASTM D792
Moisture Absorption at Equilibrium <= 0.30 %
Viscosity Test 74 - 78 cm³/gIntrinsic; ISO 1628-5
ASTM Color <= 1.0b*; ASTM D6290
 >= 64L*; ASTM D6290
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 85.0 °CASTM D3418
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 250 °C
Drying Temperature <= 70.0 °Cto avoid chips sticking together in dryer hopper
 60.0 - 65.0 °C
@Time 21600 - 28800 sec
Moisture Content <= 0.0040 %dried
Dew Point -40.0 °C
 
Descriptive Properties
Food Approval PharmacopeiaYes
Particle size320 ± 50 mg/20 chips
Pellet ShapeCylindrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSELE906 / 243404

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.