MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives 7544 Two-Component, Non-Sag, Fast-Cure Urethane Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes:
Lord Urethane Adhesives
Lord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offer primerless adhesion for sheet molded compounds (SMC) and are ideal for prepared metals, rubber, and fiber reinforced plastics (FRP). The benefits of Lord Urethane Adhesives are: Cure at Room Temperature. One-component systems can be accelerated with a catalyst. Two-component systems can be accelerated with heat. Strong, flexible bonds. They bring excellent structural integrity to assemblies made of plastic, metal, foams and elastomers. Outstanding hot strength to 250°F. ideal for meter/mix/dispense equipment. Environmentally friendly, 100% solids systems. Gravity feed. They require no special pumping equipment.

Lord Adhesives 7544 Two-Component, Non-Sag, Fast-Cure Urethane Adhesive
Two-Component, Non-Sag, Fast-Cure

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Pot Life 6.0 - 8.0 minTime before parts must be mated
 
Descriptive Properties
ViscosityLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer
RTP Company RTP 1200-90A  Polyurethane Thermoplastic Elastomer (TPU) 90 Shore A
Novatec Novablend® 7544 PVC
Lubrizol Estane® 5712 Thermoplastic Polyurethane
Lubrizol ESTANE® 5708F4 Ester Based Thermoplastic Polyurethane

PLORDAD44 / 52026

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.