MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives Autoseal U-2521NM A/B Urethane Sealant System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: LORD Autoseal® U-2521NM A/B urethane is a solvent-free, two-component urethane used for casting and laminating flexible and rigid windows, transparent adhesives and electrical potting and sealing compounds. Typical applications include safety goggles, gas mask view shields, shatter-proof coatings and safety glass laminates.

Features: provides easy casting of transparent elastomers with a variety of hardness. provides excellent adhesion to a variety of plastic and other substrates. cures to an optically clear coating; withstands UV exposure without significant change in haze or color./p> can be used on parts and devices that experience operating temperatures from -40 to +100°C (-40 to 212°F); can tolerate short term exposure up to 150°C (302°F).

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccmixed
Viscosity  50 - 200 cP
@Temperature 27.0 °C
50 - 200 cP
@Temperature 80.6 °F
U-2521NM B Hardener
 600 cP
@Temperature 27.0 °C
600 cP
@Temperature 80.6 °F
Mixed
 400 - 1000 cP
@Temperature 27.0 °C
400 - 1000 cP
@Temperature 80.6 °F
U-2521NM A Resin
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545cured; ASTM D 2240
Tensile Strength 20.0 MPa2900 psicured; ASTM D 638
Elongation at Break 200 %200 %cured; ASTM D 638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 173 µm/m-°C96.1 µin/in-°Fcured
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 15.0 °C59.0 °Fcured
 
Processing PropertiesMetricEnglishComments
Working Life 50.0 min
@Temperature 25.0 °C
50.0 min
@Temperature 77.0 °F
working life, 50 g mass, 0.3% Hg catalyst
Gel Time 25.0 min
@Temperature 25.0 °C
25.0 min
@Temperature 77.0 °F
mixed, with 0.3% Hg catalyst
Shelf Life 6.00 Month
@Temperature 21.0 - 27.0 °C
6.00 Month
@Temperature 69.8 - 80.6 °F
each component, from date of manufacture when stored in original, unopened container
 
Descriptive Properties
AppearanceClear LiquidU-2521NM A Resin
 Clear LiquidU-2521NM B Hardener
 Clear, slightly amber liquidMixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9241 / 232597

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.