Physical Properties | Metric | English | Comments |
---|
Density | 0.980 g/cc | 0.0354 lb/in³ |
| 1.15 g/cc | 0.0415 lb/in³ |
| 1.17 g/cc | 0.0423 lb/in³ |
Viscosity | 661 cP @Temperature 29.0 °C | 661 cP @Temperature 84.2 °F |
| 878 cP @Temperature 25.0 °C | 878 cP @Temperature 77.0 °F |
| 1054 cP @Temperature 22.0 °C | 1054 cP @Temperature 71.6 °F |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore D | 90 @Treatment Temp. 22.0 °C, Time 1.21e+6 sec | 90 @Treatment Temp. 71.6 °F, Time 336 hour |
Tensile Strength | 60.9 MPa @Treatment Temp. 22.0 °C, Time 1.21e+6 sec | 8840 psi @Treatment Temp. 71.6 °F, Time 336 hour |
Elongation at Break | 2.6 % @Treatment Temp. 22.0 °C, Time 1.21e+6 sec | 2.6 % @Treatment Temp. 71.6 °F, Time 336 hour |
Tensile Modulus | 3.50 GPa | 507 ksi |
Flexural Strength | 95.8 MPa @Treatment Temp. 22.0 °C, Time 1.21e+6 sec | 13900 psi @Treatment Temp. 71.6 °F, Time 336 hour |
Flexural Modulus | 3.30 GPa @Treatment Temp. 22.0 °C, Time 1.21e+6 sec | 478 ksi @Treatment Temp. 71.6 °F, Time 336 hour |
Compressive Yield Strength | 92.4 MPa @Treatment Temp. 22.0 °C, Time 1.21e+6 sec | 13400 psi @Treatment Temp. 71.6 °F, Time 336 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C @Treatment Temp. 22.0 °C, Time 1.21e+6 sec | 122 °F @Treatment Temp. 71.6 °F, Time 336 hour |
Glass Transition Temp, Tg | 50.0 °C @Treatment Temp. 22.0 °C, Time 1.21e+6 sec | 122 °F @Treatment Temp. 71.6 °F, Time 336 hour |
|
Processing Properties | Metric | English | Comments |
---|
Cure Time | 150 min @Temperature 29.4 °C | 2.50 hour @Temperature 84.9 °F |
| 225 min @Temperature 25.0 °C | 3.75 hour @Temperature 77.0 °F |
| 240 min @Temperature 22.2 °C | 4.00 hour @Temperature 72.0 °F |
Pot Life | 16.0 - 20.0 min @Load 0.150 kg, Temperature 29.0 °C | 16.0 - 20.0 min @Load 0.331 lb, Temperature 84.2 °F |
| 16.0 - 20.0 min @Load 0.500 kg, Temperature 29.0 °C | 16.0 - 20.0 min @Load 1.10 lb, Temperature 84.2 °F |
| 21.0 - 27.0 min @Load 0.500 kg, Temperature 25.0 °C | 21.0 - 27.0 min @Load 1.10 lb, Temperature 77.0 °F |
| 24.0 - 30.0 min @Load 0.150 kg, Temperature 25.0 °C | 24.0 - 30.0 min @Load 0.331 lb, Temperature 77.0 °F |
| 26.0 - 32.0 min @Load 0.500 kg, Temperature 22.0 °C | 26.0 - 32.0 min @Load 1.10 lb, Temperature 71.6 °F |
| 26.0 - 33.0 min @Load 0.150 kg, Temperature 22.0 °C | 26.0 - 33.0 min @Load 0.331 lb, Temperature 71.6 °F |
Shelf Life | 24.0 Month | 24.0 Month |
| 36.0 Month | 36.0 Month |
|
Descriptive Properties |
---|
Mix ratio | 1.96:1—2.26:1 |
| 100:41.9 |
| 100:42.9—100:37.0 |
| 100:50.0 |
| 100:51.1—100:44.2 |
| 2.00:1 |
| 2.33:1—2.70:1 |
| 2.39:1 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.