Base Polymer: Acrylonitrile/Butadiene/Styrene/Copolymer Filler/Additive System: 15% special filler Special Features: Highly reflective, opaque Market Segment: Automotive, various Application Area: lighting, light blocking components Typical Applications: light guides, reflectors Information provided by Albis Plastics |