MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

US Plastic Lumber Trimax® Structural Plastic Lumber  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic

Material Notes: Description: USPL's Structural Lumber is a high-performance construction material consisting of a patented formula of recycled plastic, fiberglass, and selected additives. The plastic raw material utilized in Structural Lumber is derived from post-consumer bottle waste such as milk and detergent bottles. This material is compounded into a consistent, reinforced plastic timber product using reactive compatibilizers, creating a strong and stable plastic/fiber matrix. Structural Lumber is a cost-effective and high-performance timber product for marine construction and commercial applications. It has exceptional resistance to marine borers, salt spray, termites, corrosive substances, oil and fuels, fungi, and other environmental stresses. It does not absorb moisture; therefore, it will not rot, splinter or crack. Structural Lumber products are manufactured in many dimensional lumber and timber sizes, particularly in large cross sections. Deck and dock planks, sheet piling, wale timbers, camels, fenders, and piles are all available from USPL. The product comes in almost any transportable length and is standard in Steel Gray. It can be special ordered in colors to complement HDPE. Structural Lumber has excellent weathering resistance; however, as with many other polyolefins, the material will fade over the service life of the product. The product requires no waterproofing, painting, staining, or similar maintenance when used in many exterior applications.

Applications: Structural Lumber products are used in a variety of commercial and marine applications and are often the product of choice for exterior applications where resistance to salt and fresh water, marine borers, and other environmentally harsh conditions is required. Due to the unique composition of USPL Structural Lumber, the product can be used for a number of structural members in commercial and shoreline timberwork. It is well suited for:

  • Dock and deck planks
  • Wale timbers
  • Sheet piling
  • Camels
  • Pilings
  • Fenders
  • Channel markers
  • Posts, beams, and joists

Information provided by U.S. Plastic Lumber (USPL).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.747 - 0.830 g/cc0.0270 - 0.0300 lb/in³ASTM D6111
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 8.62 MPa1250 psiTension Parallel to Grain; ASTM 198
Modulus of Elasticity 2.24 GPa325 ksiASTM D6109
 2.90 GPa420 ksiASTM D198
Modulus of Rupture 0.200 GPa29.0 ksiUltimate; ASTM D198 & ASTM D6109
Compressive Strength 4.83 MPa700 psiCompression Perpendicular to Grain; ASTM D143
 12.0 MPa1740 psiCompression Parallel to Grain; ASTM 198
Shear Strength 5.03 MPa730 psiParallel to grain; ASTM D143
Coefficient of Friction, Static 0.610.61Dry; Tribometer
 
Thermal PropertiesMetricEnglishComments
CTE, linear 61.2 µm/m-°C
@Temperature 20.0 °C
34.0 µin/in-°F
@Temperature 68.0 °F
ASTM D6341
 
Descriptive Properties
Screw Withdrawal380 lbsASTM D1761

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lucalen A2700M Low Density Polyethylene

PUSPL3 / 71803

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.