MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mocom (ALBIS) ALTECH® ABS A 1000/660 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Base Polymer: Acrylonitrile Butadiene Styrene Copolymer

Special Features: Injection molding grade, also suitable for extrusion, easy release (demolding)

Market Segment: Automotive, Medical/Personal Care, various

Typical Application: Kitchenware, dashboard/instrument panels, impact protection/shock absorber, various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 83.0 MPa12000 psiH358/30; ISO 2039-1
Tensile Strength, Yield 36.0 MPa5220 psiISO 527
Elongation at Break 12 %12 %ISO 527
Elongation at Yield 3.0 %3.0 %ISO 527
Tensile Modulus 1.80 GPa261 ksiISO 527
Flexural Strength 57.0 MPa8270 psiISO 178
Flexural Modulus 1.95 GPa283 ksiISO 178
Charpy Impact Unnotched  12.0 J/cm²
@Temperature -40.0 °C
57.1 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 3.30 J/cm²
@Temperature 23.0 °C
15.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °FISO 75-1/-2
Vicat Softening Point 95.0 °C203 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 260 °C428 - 500 °FInjection molding
Mold Temperature 50.0 - 80.0 °C122 - 176 °FInjection molding
Drying Temperature  80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 80.0 °C
@Time 10800 - 21600 sec
176 °F
@Time 3.00 - 6.00 hour
in an circulating dryer
 
Descriptive Properties
Base PolymerAcrylonitrile Butadiene Styrene Copolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LI970 Co-Extrusion ASA
INEOS Styrolution Luran® S 767KE Acrylonitrile Styrene Acrylate (ASA)
Bamberger Polymers Bapolan® ABS8430 ABS Polymer, Extrusion/Injection Grade

PALBIS8617 / 242676

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.